Halogen-free High Reliability Solder Paste based on SABI alloy

  • SB6N58-HF350
Halogen-free High Reliability Solder Paste based on SABI alloy

SB6N is a high-reliability alloy that reduces solder joint transformation through advanced alloy strengthening technologies. The addition of indium significantly enhances the thermomechanical durability of the solder joints. With excellent thermal fatigue properties, SB6N is ideal for harsh conditions, improving product life in automotive and industrial equipment. Additionally, its lower melting point compared to SAC305 allows for reduced reflow temperatures.

feature

  • Effectively suppresses crack extension under thermal cycle conditions
  • Significantly reduces voiding
  • Enables to use the same reflow profile as SAC305
  • Applicable for 0603 metric chips / 0.25 mm diameter for CSP mounting
  • Halogen free, no artificial addition of any halogen element

Product Performance Table

  • Product name

    SB6N58-HF350

  • Composition

    Sn 3.5Ag 0.5Bi 6.0In

  • Melting Point(℃)

    202 - 210

  • Particle Size(μm)

    20 - 38

  • Flux Content(%)

    11.0

  • Viscosity(Pa.s)

    200

  • Halide content(%)

    0

  • Flux Type

    ROL0 (IPC J-STD-004B)

Increasing Demand for Reliability

PCBs in an electric product for automotive or industrial equipment are exposed to harsh working environments with significant temperature differences and in some cases, SAC305 solder alloy cannot provide sufficient reliability.
Temperature cycling causes stress in the solder joint due to the components and PCB to expansion and contraction, and the stress causes cracking in the solder joint.

Therefore, a solder alloy which withstands thermal-cycle stress is required.

Alloy Strengthening by In and Bi addition (Solid Solution Strengthening) 

Dislocations (irregularities in the crystal structure) occur in metals including Tin (Sn), the bulk material of the solder. Dislocations eventually cause plastic deformation and cracking in the solder joint. Bi and In do not form compounds with Sn but replace the Sn atoms in their lattice positions (form a solid solution). As the atomic radius of Bi and In are significantly larger than Sn, they form distortions within the matrix which prevent propagation and accumulation of dislocations. In addition, this alloy has a lower melting point than SAC305 and reduces the thermal stress to the components during reflow.

Prevents cracking from thermal-cycle stress

Solid solution strengthening offers high thermal-fatigue resistance as it does not fail even in a harsh temperature condition, such as -40˚C ~+150˚C.

Thermal-fatigue resistance contributes to an extension of product life of automotive electronics, failure of which may result in safety issues and for industrial equipment the product is expected to be longer-lasting.

Solve the Issues Associated with a Halogen-Free Product with Flux Technology

The flux in SB6N58-HF350 is designed to prevent activation not only in storage but also the preheat stage of reflow so that it can perform its full activation during the reflow stage.