KOKI COMPANY LIMITED KOKI COMPANY LIMITED

  1. ホーム
  2. Products
  3. Solder Paste
  4. Halogen-free High Reliability Solder Paste based on SABI alloy applicable for ENIG plating

Halogen-free High Reliability Solder Paste based on SABI alloy applicable for ENIG plating

  • SB6NX58-HF350
Halogen-free High Reliability Solder Paste based on SABI alloy applicable for ENIG plating

SB6NX is a high-reliability alloy that reduces solder joint transformation through advanced alloy strengthening technologies. The addition of indium significantly enhances the thermomechanical durability of the solder joints. With excellent thermal fatigue properties, SB6NX is ideal for harsh conditions, improving product life in automotive and industrial equipment. Additionally, its lower melting point compared to SAC305 allows for reduced reflow temperatures. It is applicable for any surface finishes of the PCB, including ENIG.

feature

  • Effectively suppresses crack extension under thermal cycle conditions
  • SB6NX alloy is applicable for any surface finishes of the PCB, including ENIG
  • Significantly reduces voiding
  • Enables to use the same reflow profile as SAC305
  • Halogen free, no artificial addition of any halogen element

Product Performance Table

  • Product name

    SB6NX58-HF350

  • Composition

    Sn 3.5Ag 0.5Bi 6.0In 0.8Cu

  • Melting Point(℃)

    202 - 204

  • Particle Size(μm)

    20 - 38

  • Flux Content(%)

    10.8 / 12.5( for Dispense)

  • Viscosity(Pa.s)

    200 / 120( for Dispense)

  • Halide content(%)

    0

  • Flux Type

    ROL0 (IPC J-STD-004B)

  • Characteristics

    for Dispense : SB6NX58-HF350D

Increasing Demand for Reliability

PCBs in an electric product for automotive or industrial equipment are exposed to harsh working environments with significant temperature differences and in some cases, SAC305 solder alloy cannot provide sufficient reliability.
Temperature cycling causes stress in the solder joint due to the components and PCB to expansion and contraction, and the stress causes cracking in the solder joint.

Therefore, a solder alloy which withstands thermal-cycle stress is required.

Alloy Strengthening by In and Bi addition (Solid Solution Strengthening)

Dislocations (irregularities in the crystal structure) occur in metals including Tin (Sn), the bulk material of the solder. Dislocations eventually cause plastic deformation and cracking in the solder joint. Bi and In do not form compounds with Sn but replace the Sn atoms in their lattice positions (form a solid solution). As the atomic radius of Bi and In are significantly larger than Sn, they form distortions within the matrix which prevent propagation and accumulation of dislocations. In addition, this alloy has a lower melting point than SAC305 and reduces the thermal stress to the components during reflow.

Prevents cracking from thermal-cycle stress

Solid solution strengthening offers high thermal-fatigue resistance as it does not fail even in a harsh temperature condition, such as -40˚C ~+150˚C.

Thermal-fatigue resistance contributes to an extension of product life of automotive electronics, failure of which may result in safety issues and for industrial equipment the product is expected to be longer-lasting.

Compatible with ENIG Finish Soldering Pads

Sn-Ni based IMC layer grows in the ENIG finish pad (Au plating layer of the soldering pad) and forms a Phosphorus (P)-rich layer which makes the solder joint interface brittle.

SB6NX solder alloy contains Cu, which is highly compatible with Ni, and forms a barrier layer to prevent Ni diffusion. As a result, the combination of SB6NX solder and the ENIG finish pad can obtain equivalent joint reliability as OSP the finish pad.

フラックス技術でハロゲンフリーの課題を解決

SB6NX58-HF350のフラックスは、保管中だけでなく、予熱段階でも反応を抑えるように設計しており、
はんだ溶融時に最大限の効果を発揮します。

Keywords / Related Products

The specified post was not found.

Contact Us

Requests for estimates, requests for materials/catalogs, consultations on new installations, etc.
Please feel free to contact us.